Sorry, the search criteria can not be empty
Search
View All Categories
Seasonal Sale! As usual see

Conductive Silver Ink forms electronic circuits with UV light

04/17/2013 21:13:59

After printing circuit on base material using Conductive Silver Ink and exposing it to UV light for 0.3 seconds, user can instantly harden printed film at room temperature to form circuit. At film thickness of 5 µm or more, it is possible to form wiring with electrical resistivity of 10-3 cmW. Wiring can be formed on glass base material and substrates as well as flexible base materials such as PVC film and PET film.